Polymer Property : Film Tensile Strength at Break, MD = 7060 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 48.7 - 52.7 MPa
7060 - 7640 psi
3M 6147 Performance Reinforced Water Activated Tape
3M™ Performance Reinforced Water Activated Tape 6147 is used for box sealing and other packaging applications. This has a fiberglass reinforced paper backing and a high tack water activated adhesiv..