Polymer Property : Film Tensile Strength at Break, MD = 6470 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 44.6 MPa
6470 psi
Calculated from mfr's report of 229 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® E56 Paper, 20 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Film Tensile Strength at Break, MD 44.6 MPa
6470 psi
ASTM D882
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g..