Film Tensile Strength at Break, MD 60.8 MPa
8820 psi
ASTM D882
Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: processing aid additiveCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blended with LDPE or HDPEApplications: thick or t..