Film Tensile Strength at Break, MD 40.7 MPa
5900 psi
ASTM D882
Westlake LF2020 Hexene Linear Low Density Polyethylene
Westlake LF2020 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..
Film Tensile Strength at Break, MD 40.7 MPa
5900 psi
ASTM D882
Dow ELITE™ 5230G Enhanced Polyethylene Resin
™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, th..
Film Tensile Strength at Break, MD >= 40.7 MPa
>= 5900 psi
ASTM D 882A
Total Finathene® HL 328 HDPE resin  (discontinued **)
Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by ..