Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 25.0 - 57.0 MPa
3630 - 8270 psi
Average value: 47.0 MPa Grade Count:6
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..