Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 37.0 - 317 MPa
5370 - 46000 psi
Average value: 96.7 MPa Grade Count:16
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..