Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 41.5 MPa | 6020 psi | ASTM D882 |
Eastman Eastman AP007 Copolyester Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an.. |
|||
Film Tensile Strength at Break, MD | 41.5 MPa | 6020 psi | |
Dow AFFINITY™ PL 1850 Polyolefin Plastomer AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistanc.. |