Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 269 - 379 MPa | 39000 - 55000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OMBS (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Medium Barrier is a 0.60 mil (15 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug.. |
|||
Film Tensile Strength at Break, MD | 269 - 379 MPa | 39000 - 55000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OMBS (1.00 mil) Monoaxially Oriented, Co-Extruded Nylon 6-Based Clear Film Description: Oxyshield™ Oriented Medium Barrier is a 1.00 mil (25 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug.. |
|||
Film Tensile Strength at Break, MD | 269 MPa | 39000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 0.6 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of .. |