Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 38.2 MPa | 5540 psi | |
Kuraray HYBRAR® CF1 Mono Layer Cast Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Film Tensile Strength at Break, MD | 38.2 MPa | 5540 psi | |
Kuraray HYBRAR® CF4 Mono Layer Cast Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |