Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 255 MPa | 37000 psi | ASTM D882-67 (Modified to TDF) |
DuPont Teijin Films Teonex® Q72 Polyester Film, 14 Gauge Teonex® Q72 is biaxially oriented, slightly hazy polyethylene naphthalate (PEN) film. This ultra thin film which was developed for capacitor applications. It is commercially available in nominal 14.. |