Film Tensile Strength at Break, MD 35.3 MPa
5120 psi
Kuraray HYBRAR® CF2 Mono Layer Cast Film
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..