Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 23.9 MPa
3470 psi
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade
DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl..