Polymer Property : Film Tensile Strength at Break, MD = 3272 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD >= 22.56 MPa
>= 3272 psi
ASTM D882
Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.