Polymer Property : Film Tensile Strength at Break, MD = 3150 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 21.7 MPa
3150 psi
ASTM D882
LG Chemical LUTENE FB0800 LDPE Blown Film
Description: LUTENE FB0800 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of greenhouse film. LUTENE FB0800 have the excellent mechanical proper..