Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, MD = 241 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 241 - 296 MPa
35000 - 43000 psi
ASTM D882
Honeywell Capran® Emblem™ 1000 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ 1000 is a 0.40 mil (10 micron) biaxially oriented nylon 5 film with excellent flex crack resistance and superior clarity properties. Applications: packaging appl..
Film Tensile Strength at Break, MD 241 MPa
35000 psi
ASTM D882
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 1.0 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of ..
Film Tensile Strength at Break, MD 241 MPa
35000 psi
Orientation not specified; ASTM D882
DuPont™ Kapton® 100KN Polyimide Film, 25 Micron Thickness
Film thickness 25 micron (1.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian..
Film Tensile Strength at Break, MD 241 MPa
35000 psi
Orientation not specified; ASTM D882
DuPont™ Kapton® 300KN Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian..
Film Tensile Strength at Break, MD 241 MPa
35000 psi
Orientation not specified; ASTM D882
DuPont™ Kapton® 200KN Polyimide Film, 50 Micron Thickness
Film thickness 50 micron 2.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianh..
Film Tensile Strength at Break, MD 241 MPa
35000 psi
ASTM D882A
DuPont Teijin Films Melinex® HS2 Polyester Film
Melinex® HS2 is a low TD shrinkage, low neckdown polyester film with excellent handling properties. It is ideal for the hot stamping marketInformation provided by DuPont.
Copyright © lookpolymers.com All Rights Reserved