Polymer Property : Film Tensile Strength at Break, MD = 23.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 23.3 MPa
3380 psi
50 µm (2 mil) film; ASTM D882
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res..