Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 137 MPa | 19900 psi | ExxonMobil Method |
ExxonMobil Bicor® 100 AB-X OPP Film Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as.. |
|||
Film Tensile Strength at Break, MD | 137 MPa | 19900 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 310 AB OPP Film Product Description: Bicor AB is a two-side acrylic coated, sealable OPP film designed for general use in applications, including overwrap, horizontal, and vertical packaging. This film is suitable .. |