Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 124.97 MPa | 18125 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® HS Polyester Film, 1400 Gauge Teijin® Tetoron® HS is a very clear polyester film. It is available in a wide range of thicknesses.Typical Applications: OHP SheetLabelsITOLaminated CardsWindow FilmInformation provided by DuPont.. |