Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 176.0 MPa | 25520 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® HSL Polyester Film, 740 Gauge Teijin® Tetoron® HSL is a low shrinkage polyester film with well balanced physical, chemical and optical properties. In addition to the standard, non-pretreated, Teijin® Tetoron® HSL film, the f.. |
|||
Film Tensile Strength at Break, MD | 176.0 MPa | 25520 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 150 Gauge Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhe.. |
|||
Film Tensile Strength at Break, MD | 176.0 MPa | 25520 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 200 Gauge Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhe.. |
|||
Film Tensile Strength at Break, MD | 176.0 MPa | 25520 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 300 Gauge Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhe.. |
|||
Film Tensile Strength at Break, MD | 176.0 MPa | 25520 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 400 Gauge Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhe.. |
|||
Film Tensile Strength at Break, MD | 176.0 MPa | 25520 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 300 Gauge Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod.. |