Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 78.0 MPa | 11300 psi | ASTM D882 |
Braskem ES 300 HDPE Blown Film Extrusion Polyethylene
(discontinued **) 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags; high-strength films. Informa.. |
|||
Film Tensile Strength at Break, MD | 77.911 MPa | 11300 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |