Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 76.60 MPa | 11110 psi | ASTM D882 |
ExxonMobil Exceed™ 3512CB Film Resin Exceed 3512CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3512CB resin have outstanding cold temperature toughness, impact strength and punc.. |