Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 71.64 MPa | 10390 psi | ASTM D882 |
ExxonMobil Exceed™ 1012CA Film Resin
(discontinued **) Exceed 1012CA mVLDPE resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1012CA resin have outstanding cold temperature toughness, impact strength a.. |