Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 902 g | 902 g | ASTM D1922 |
Dow DOWLEX™ 2045G Linear Low Density Polyethylene DOWLEX™ 2045G resin is designed for the production of a wide variety of industrial and consumer films (though it is not recommended for silage stretch film). The product also delivers very good pr.. |