Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 80.0 - 550 g
80.0 - 550 g
Average value: 235 g Grade Count:11
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is ..