Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 69 g | 69 g | ASTM D1922 |
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Elmendorf Tear Strength MD | 69 g | 69 g | ASTM D1922 |