Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 675 g | 675 g | ASTM D1922 |
Dow FLEXOMER™ ETS-9066 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |