Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 63 g | 63 g | ASTM D 1922 |
NOVA Chemicals Novapol® PF-0318-E Butene LLDPE Film Resin PF-0318-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |