Polymer Property : Elmendorf Tear Strength MD = 460 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 460 g
460 g
ASTM D1922
M. Holland Company MAGMA® LL1091-K LLDPE  (discontinued **)
Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Elmendorf Tear Strength MD 460 g
460 g
ASTM D1922
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin
Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America..
Elmendorf Tear Strength MD 460 g
460 g
Dow LDPE 586A Low Density Polyethylene, Packaging Grade
DOW LDPE 586A resin is used for general purpose packaging applications. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulatio..
Elmendorf Tear Strength MD 460 g
460 g
ASTM D1922
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali..
Elmendorf Tear Strength MD 460 g
460 g
ASTM D1922
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.Applications: Sealing layer in coextr..
Elmendorf Tear Strength MD 460 g
460 g
ASTM D638
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr..