Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 438 g | 438 g | ASTM D1922 |
Dow DOWLEX™ 2056G Linear Low Density Polyethylene Improved thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |