Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 178 g
178 g
Dow AFFINITY™ PL 1845 Polyolefin Plastomer
Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.