Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 12.0 - 1080 g | 12.0 - 1080 g | Average value: 237 g Grade Count:115 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Elmendorf Tear Strength MD | 12.0 - 64.0 g | 12.0 - 64.0 g | Average value: 43.7 g Grade Count:3 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |