Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 1080 g
1080 g
3 mil; ASTM D1922
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin
Features: Moderate toughness and strengthGood stiffnessEasy processabilityExcellent seal properties Applications: Heavy duty shipping sacks requiring moderate toughness and high stiffnessIndustrial ..