Secant Modulus 0.0531 - 1.05 GPa
7.70 - 152 ksi
Average value: 0.601 GPa Grade Count:6
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..