Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 4.80 GPa | 696 ksi | ASTM D882 |
DuPont™ Kapton® 100EN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |
|||
Secant Modulus | 4.80 GPa | 696 ksi | ASTM D882 |
DuPont™ Kapton® 50EN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |