Polymer Property : Secant Modulus = 4.019 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.02771 GPa
4.019 ksi
ASTM D412 Method A
Seals Eastern 7265 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Vito..