Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.750 - 1.54 GPa | 109 - 224 ksi | Average value: 1.06 GPa Grade Count:26 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |