Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.0121 GPa | 1.75 ksi | ASTM D412 Method A |
Seals Eastern 7182D Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |