Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.480 GPa | 69.6 ksi | 1% Secant Modulus; Non-oriented Film; ASTM D882 |
Total PPR 8473 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8473 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The very .. |
|||
Secant Modulus | 0.480 - 0.793 GPa | 69.6 - 115 ksi | Average value: 0.625 GPa Grade Count:17 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |