Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.01573 GPa | 2.282 ksi | ASTM D412 Method A |
Seals Eastern 7182X Fluorocarbon-Elastomer Formulated AFLAS®. Ultra-low compressive stress relaxation for alkaline, high-temperature service.Information provided by Seals Eastern, Inc. |