Polymer Property : Film Tensile Strength at Yield, MD = 9.549 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.549 MPa
1385 psi
ASTM D882
Dow ELITE™ 5230G Enhanced Polyethylene Resin
™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, th..