Polymer Property : Film Tensile Strength at Yield, MD = 9.218 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.218 MPa
1337 psi
ASTM D882
Dow DOWLEX™ 2267G Linear Low Density Polyethylene
A high performance stretch film resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow