Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 62.0 MPa | 8990 psi | ASTM-D882 |
Westlake Mxsten CV77519 Polyethylene Plastomer Mxsten CV Plastomer CV77519 is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock. It does contain high processing aid. Films produced with this resin .. |