Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 51.7 MPa
7500 psi
ASTM D882
Formosa Plastics Formolene® E905 Film HDPE  (discontinued **)
HMW-Bimodal ResinApplications: T-shirt bags, trash can liners, heavy duty bagsFormolene E905 is a high molecular weight grade of HDPE with well-balanced strength in both the machine (MD) and transve..