Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 5.00 - 68.3 MPa | 725 - 9910 psi | Average value: 12.5 MPa Grade Count:11 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |