Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | >= 44.0 MPa | >= 6380 psi | ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Film Tensile Strength at Yield, MD | >= 44.0 MPa | >= 6380 psi | ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Film Tensile Strength at Yield, MD | 44.0 MPa | 6380 psi | ASTM D882 |
Braskem Flexus® 9210 LLDPE Blown Film Extrusion
(discontinued **) 25µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); multilayer packaging films; films for lamination. Information provided by Braskem |
|||
Film Tensile Strength at Yield, MD | 44.0 MPa | 6380 psi | ASTM D828 |
DuPont™ Nomex® Type 993, 95 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |