Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 43.0 MPa | 6240 psi | ASTM D882 |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Film Tensile Strength at Yield, MD | 43.0 MPa | 6240 psi | ASTM D882 |
Eastman Embrace LV Copolyester for Shrink Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Film Tensile Strength at Yield, MD | 43.0 MPa | 6240 psi | ASTM D882 |
Eastman Tritan FX200 Copolyester Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Film Tensile Strength at Yield, MD | 43.0 MPa | 6240 psi | ASTM D882 |
Braskem HF 0147 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |