Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 52.4 MPa
7600 psi
ASTM D638
Wanshijie APET Sheet
APET sheet is one of the earliest plastic sheets our company develops and produces. It has excellent air-tightness, durability, chemical resistance and transparency. When burnt, it will not produce ..