Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 3.45 MPa | 500 psi | ASTM D882 |
ExxonMobil EXACT™ 4056 Plastomer for Film Blends and Blown Film Applications Product Description: Exact 4056 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin can be used in blends with polyolefins to improve.. |