Film Tensile Strength at Yield, MD 32.4 MPa
4700 psi
ASTM D882
Honeywell Stretch-Vac® 2000 Heat-Stabilized Blown Film  (discontinued **)
Description: Stretch-Vac® 2000 is a pink tinted, high elongation, heat-stabilized blown film produced from modified polyamide resin. It is available in widths up to 80 inches as layflat tubing and..
Film Tensile Strength at Yield, MD 32.4 MPa
4700 psi
ASTM D882
Honeywell Stretch-Vac® Elastomax 1000 Heat-Stabilized Blown Film  (discontinued **)
Description: Capran® Elastomax 1000 is a pink tinted, heat-stabilized blown film produced from modified nylon resin. It is available in widths up to 80 inches as layflat tubing and 120 inches as s..