Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 40.7 MPa | 5900 psi | ASTM D882 |
ExxonMobil HDPE HTA 001HD High Density Polyethylene (HMW) Resin Product Description: HTA 001HD is a high weight HDPE film grade. Films made from HTA 001HD exhibit excellent impact and toughness properties as well as high stiffness. Availability: Africa & Middle .. |
|||
Film Tensile Strength at Yield, MD | 40.7 MPa | 5900 psi | ASTM D882 |
ExxonMobil HDPE HTA 001HP2 High Density Polyethylene (HMW) Resin Product Description: HTA 001HP2 is a high molecular weight HDPE film grade providing very good processability on high output extruders. Films made from HTA 011HP2 exhibit excellent impact and toughn.. |